Fig. 4From: Magnetic hyperthermia enhance the treatment efficacy of peri-implant osteomyelitisCharacteristics of Fe3O4 nanoparticles. a The XRD pattern of the Fe3O4 nanoparticles. b Room-temperature magnetization curves for FO111019-P and FO111019-h. Magnetic hysteresis curves measured at room temperature for the samples prepared by a hydrothermal process (square: FO111019-h, dot: FO111019-p) showed the super-paramagnetic characteristics. c The crystal structure of Fe3O4 nanoparticles prepared at the injection temperature of 290 °C (TEM). The average diameter of particles is 16 nmBack to article page